25MnTiBRE
25MnTiBRE is a grade designated under GB. Its recorded composition includes C 0.22–0.28%, Si 0.2–0.45%, Cr ≤ 0.3%, Mn 0.3–1.6% and Ni ≤ 0.3%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include Rm ≥ 1380 N/mm², A ≥ 10% and HB 229.
- Designations 1
Chemical composition
11 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.22–0.28 | |
0.2–0.45 | |
0.3–1.6 | |
≤ 0.03 | |
≤ 0.03 | |
≤ 0.3 | |
≤ 0.1 | |
≤ 0.3 | |
≤ 0.3 | |
0.04–0.1 | |
0.0008–0.0035 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| B | 0.0008-0.0035 | 0.001 | 0.004 | Range |
| C | 0.22-0.28 | 0.220 | 0.280 | Range |
| Si | 0.2-0.45 | 0.200 | 0.450 | Range |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.03 | — | 0.030 | Max |
| Ti | 0.04-0.1 | 0.040 | 0.100 | Range |
| Cr | ≤0.3 | — | 0.300 | Max |
| Mn | 0.3-1.6 | 0.300 | 1.600 | Range |
| Ni | ≤0.3 | — | 0.300 | Max |
| Cu | ≤0.3 | — | 0.300 | Max |
| Mo | ≤0.1 | — | 0.100 | Max |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
computed from composition · °CThese four temperatures are a CALCULATION from this grade's own composition, using the published Li, Niebuhr, Meekisho & Atteridge (1998) model — never a measurement, and computed from the UPPER BOUND of each element's specified range, not a mid-range figure. Where this grade also has a measured transformation point (Ac1, Ac3, Ar1, Ar3) on file, it is shown separately, in Physical & mechanical properties, and is never replaced by the predicted figures here — Ae (predicted, equilibrium) and Ac/Ar (measured, on heating or cooling) are different physical quantities and can differ by tens of degrees; a mismatch between the two is not an error in either.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values4 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
Supply condition
- Quenching
- Carburizing
- Quenching and TemperingTest specimen
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.