| Grade | Material no. | Category | Designations | C% | Si% | Mn% | S% | Cr% |
|---|---|---|---|---|---|---|---|---|
| G28Mn6 | 1.11651.1 | Quenched and tempered steels | 56 | 0,25-0,32 | ≤0,60 | 1,20-1,80 | 0,03 | — |
| 1.1167 | 1.11671.1 | Quenched and tempered steels | 82 | 0,32-0,40 | ≤0,40 | 1,20-1,50 | 0,035 | — |
| 1.1170 | 1.11701.1 | Quenched and tempered steels | 44 | 0,25-0,32 | ≤0,40 | 1,30-1,65 | 0,035 | ≤0,40 |
| 30Mn5 | 1.11731.1 | Quenched and tempered steels | 10 | 0,27-0,34 | 0,15-0,40 | 1,20-1,50 | 0,035 | ≤0,30 |