4Cr5MoWVSi
4Cr5MoWVSi is a grade designated under GB. Its recorded composition includes C 0.32–0.4%, Si 0.8–1.2%, Cr 4.75–5.5%, Mo 1.25–1.6% and W 1.1–1.6%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HB ≤ 235.
- Designations 1
Chemical composition
10 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.32–0.4 | |
0.8–1.2 | |
0.2–0.5 | |
≤ 0.025 | |
≤ 0.02 | |
4.75–5.5 | |
1.25–1.6 | |
0.2–0.5 | |
1.1–1.6 | |
≤ 0.25 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.32-0.4 | 0.320 | 0.400 | Range |
| Si | 0.8-1.2 | 0.800 | 1.200 | Range |
| P | ≤0.025 | — | 0.025 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 0.2-0.5 | 0.200 | 0.500 | Range |
| Cr | 4.75-5.5 | 4.750 | 5.500 | Range |
| Mn | 0.2-0.5 | 0.200 | 0.500 | Range |
| Cu | ≤0.25 | — | 0.250 | Max |
| Mo | 1.25-1.6 | 1.250 | 1.600 | Range |
| W | 1.1-1.6 | 1.100 | 1.600 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values1 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 1299-2025
- Quenching1000–1030 °CQuenchant Oil or Air
Supply condition
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.