6W6Mo5Cr4V
6W6Mo5Cr4V is a grade designated under GB. Its recorded composition includes C 0.55–0.65%, V 0.7–1.1%, Cr 3.7–4.3%, Mo 4.5–5.5% and W 6–7%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HB ≤ 269.
- Designations 1
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.55–0.65 | |
≤ 0.4 | |
≤ 0.6 | |
≤ 0.03 | |
≤ 0.02 | |
3.7–4.3 | |
4.5–5.5 | |
0.7–1.1 | |
6–7 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.55-0.65 | 0.550 | 0.650 | Range |
| Si | ≤0.4 | — | 0.400 | Max |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 0.7-1.1 | 0.700 | 1.100 | Range |
| Cr | 3.7-4.3 | 3.700 | 4.300 | Range |
| Mn | ≤0.6 | — | 0.600 | Max |
| Mo | 4.5-5.5 | 4.500 | 5.500 | Range |
| W | 6-7 | 6.000 | 7.000 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values1 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 1299-2025
- Quenching1180–1200 °CCooling Oil
Supply condition
- QuenchingTest specimen
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.
Source: www.caishuku.com
Looking for this grade under another name?