9Cr3MoV
9Cr3MoV is a grade designated under GB. Its recorded composition includes C 0.85–0.95%, Si 0.25–0.45%, Cr 2.5–3.5%, Mn 0.2–0.35% and Mo 0.2–0.4%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HB ≤ 255.
- Designations 1
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.85–0.95 | |
0.25–0.45 | |
0.2–0.35 | |
≤ 0.02 | |
≤ 0.015 | |
2.5–3.5 | |
0.2–0.4 | |
≤ 0.25 | |
0.1–0.2 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.85-0.95 | 0.850 | 0.950 | Range |
| Si | 0.25-0.45 | 0.250 | 0.450 | Range |
| P | ≤0.02 | — | 0.020 | Max |
| S | ≤0.015 | — | 0.015 | Max |
| V | 0.1-0.2 | 0.100 | 0.200 | Range |
| Cr | 2.5-3.5 | 2.500 | 3.500 | Range |
| Mn | 0.2-0.35 | 0.200 | 0.350 | Range |
| Ni | ≤0.25 | — | 0.250 | Max |
| Mo | 0.2-0.4 | 0.200 | 0.400 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
This grade's composition falls outside the published model's validated range (a low-alloy composition window), so no transformation temperature is predicted here.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values1 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 1299-2025
- Quenching890–950 °CQuenchant Air or Oil
Supply condition
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.