CW6Mo5Cr4V3
CW6Mo5Cr4V3 is a designation in GB for the grade also listed as HS6-5-3. We list 5 designations recorded for this grade, in the standards DIN / EN, ISO, JIS, GB and KS.
- Designations 5
Also known as
5 designations · 5 standards · nothing hidden- CW6Mo5Cr4V3This grade’s own name
Every designation on file is listed — no truncation, no “+ n more”. Each one is itself a route that leads back here.
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
1.25–1.32 — | |
≤ 0.7 | |
0.15–0.4 | |
≤ 0.03 | |
≤ 0.02 | |
3.75–4.5 | |
4.7–5.2 | |
2.7–3.2 — | |
5.9–6.7 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 1.25-1.32 | 1.250 | 1.320 | Range |
| Si | ≤0.7 | — | 0.700 | Max |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 2.7-3.2 | 2.700 | 3.200 | Range |
| Cr | 3.75-4.5 | 3.750 | 4.500 | Range |
| Mn | 0.15-0.4 | 0.150 | 0.400 | Range |
| Mo | 4.7-5.2 | 4.700 | 5.200 | Range |
| W | 5.9-6.7 | 5.900 | 6.700 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values3 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 9943-2025
- Preheating800–900 °C
- Quenching1180–1200 °CQuenchant Oil, Salt bath or Nitrogen
- Tempering550 °C
Supply condition
- AnnealingSupply condition
- Quenching and TemperingTest specimen
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.
Source: www.caishuku.com