W2Mo9Cr4V2 is a grade designated under GB. Its recorded composition includes C 0.95–1.05%, V 1.75–2.2%, Cr 3.5–4.5%, Mo 8.2–9.2% and W 1.5–2.1%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HB 255–302; these figures vary with the delivery condition and dimension.
- Designations 1
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.95–1.05 | |
≤ 0.7 | |
0.15–0.4 | |
≤ 0.03 | |
≤ 0.02 | |
3.5–4.5 | |
8.2–9.2 — | |
1.75–2.2 — | |
1.5–2.1 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.95-1.05 | 0.950 | 1.050 | Range |
| Si | ≤0.7 | — | 0.700 | Max |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 1.75-2.2 | 1.750 | 2.200 | Range |
| Cr | 3.5-4.5 | 3.500 | 4.500 | Range |
| Mn | 0.15-0.4 | 0.150 | 0.400 | Range |
| Mo | 8.2-9.2 | 8.200 | 9.200 | Range |
| W | 1.5-2.1 | 1.500 | 2.100 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values3 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 9943-2025
- Preheating800–900 °C
- Quenching1190–1210 °CQuenchant Oil, Salt bath or Nitrogen
- Tempering550 °C
Supply condition
- AnnealingSupply condition
- AnnealingSupply condition
- Quenching and TemperingTest specimen
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.