W3Mo3Cr4V2
W3Mo3Cr4V2 is a designation in GB for the grade also listed as HS3-3-2. We list 2 designations recorded for this grade, in the standards ISO and GB.
- Designations 2
Also known as
2 designations · 2 standards · nothing hidden- W3Mo3Cr4V2This grade’s own name
Every designation on file is listed — no truncation, no “+ n more”. Each one is itself a route that leads back here.
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.95–1.03 | |
≤ 0.45 | |
0.2–0.4 | |
≤ 0.03 | |
≤ 0.02 | |
3.8–4.5 | |
2.5–2.9 | |
2.2–2.5 — | |
2.7–3 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.95-1.03 | 0.950 | 1.030 | Range |
| Si | ≤0.45 | — | 0.450 | Max |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 2.2-2.5 | 2.200 | 2.500 | Range |
| Cr | 3.8-4.5 | 3.800 | 4.500 | Range |
| Mn | 0.2-0.4 | 0.200 | 0.400 | Range |
| Mo | 2.5-2.9 | 2.500 | 2.900 | Range |
| W | 2.7-3 | 2.700 | 3.000 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values2 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 9943-2025
- Preheating800–900 °C
- Quenching1170–1190 °CQuenchant Oil, Salt bath or Nitrogen
- Tempering550 °C
Supply condition
- Quenching and TemperingTest specimen
- AnnealingSupply condition
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.
Source: www.caishuku.com