W9Mo3Cr4V
W9Mo3Cr4V is a grade designated under GB. Its recorded composition includes C 0.77–0.87%, V 1.3–1.7%, Cr 3.8–4.4%, Mo 2.7–3.3% and W 8.5–9.5%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HB 255–269; these figures vary with the delivery condition and dimension.
- Designations 1
Chemical composition
9 elements on file · weight %What this alloy is
Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.
| Element | % by weight |
|---|---|
0.77–0.87 | |
0.2–0.4 | |
0.2–0.4 | |
≤ 0.03 | |
≤ 0.02 | |
3.8–4.4 | |
2.7–3.3 | |
1.3–1.7 | |
8.5–9.5 |
The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.
| Element | As publishedsource text, verbatim | Min% by weight | Max% by weight | Bound |
|---|---|---|---|---|
| C | 0.77-0.87 | 0.770 | 0.870 | Range |
| Si | 0.2-0.4 | 0.200 | 0.400 | Range |
| P | ≤0.03 | — | 0.030 | Max |
| S | ≤0.02 | — | 0.020 | Max |
| V | 1.3-1.7 | 1.300 | 1.700 | Range |
| Cr | 3.8-4.4 | 3.800 | 4.400 | Range |
| Mn | 0.2-0.4 | 0.200 | 0.400 | Range |
| Mo | 2.7-3.3 | 2.700 | 3.300 | Range |
| W | 8.5-9.5 | 8.500 | 9.500 | Range |
The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.
Predicted transformation temperatures
Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.
Physical & mechanical properties
An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.
Properties by condition
0 conditions · 0 values3 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.
Heat treatment
GB /T 9943-2025
- Preheating800–900 °C
- Quenching1210–1230 °CQuenchant Oil, Salt bath or Nitrogen
- Tempering550 °C
Supply condition
- AnnealingSupply condition
- Quenching and Tempering
- AnnealingSupply condition
Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.
Source: www.caishuku.com
Looking for this grade under another name?
Search the catalogue by designation, material number or composition — every name on this page is itself a way in.