Every grade designated under GOST, with the material number it maps to, what kind of steel it is, its carbon window and how many other standards carry it. Open a grade for its full composition, properties and its designations in other standards. Unless marked, every name here is an indicative cross-reference, not an asserted identity — the grades are close, not interchangeable. 3 of 50 rows differ and carry a “This grade’s own name” mark.
Also known as
3544 designations| Grade | Material no. | Category | C% by weight | Also inother standards |
|---|---|---|---|---|
| 12KhN3A | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12KhN3A-sh | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12KhN3A-sh | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12KHN3А | 1.5732 | Case hardening steels | 0.1–0.17 | 13 |
| 12KhNVFA | — | — | — | — |
| 12MKh | 1.7335 | Heat-resistant structural steels | 0.08–0.18 | 22 |
| 12X13 This grade’s own name | — | — | — | 3 |
| 12X17 | 1.4016 | Stainless steels | ≤ 0.08 | 18 |
| 12X18H10T | 1.4878 | Heat resistant steels | ≤ 0.1 | 14 |
| 12X1MΦ This grade’s own name | — | — | — | 1 |
| 12X2M | 1.7380 | Heat-resistant structural steels | 0.08–0.14 | 20 |
| 12XH3A-ш | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12XH3A-ш | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12XM | 1.7335 | Heat-resistant structural steels | 0.08–0.18 | 22 |
| 12XН3А | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12XН3А | 1.5752 | Case hardening steels | 0.14–0.2 | 15 |
| 12Г2 | — | — | 0.08–0.17 | — |
| 12Г2Б | — | — | 0.1–0.16 | — |
| 12Г2СМФ | — | — | 0.09–0.15 | — |
| 12ГН2МФАЮ | — | — | 0.09–0.16 | — |
| 12ГФ | — | — | — | — |
| 12ДН2ФЛ | — | — | 0.08–0.16 | — |
| 12К This grade’s own name | — | — | — | — |
| 12К | 1.0345 | Heat-resistant structural steels | ≤ 0.16 | 18 |
| 12Х1 | 1.2063 | Tool steels for cold work | 1.4–1.6 | 4 |
| 12Х11В2МФ | — | — | 0.09–0.14 | — |
| 12Х12М1БФР | — | — | 0.1–0.15 | — |
| 12Х12М1БФР-Ш | — | — | 0.1–0.15 | — |
| 12Х12МВФБР | — | — | 0.1–0.15 | — |
| 12Х13 | 1.4006 | Stainless steels | 0.08–0.15 | 26 |
| 12Х14Н14В2М | — | — | ≤ 0.15 | — |
| 12Х17 | 1.4016 | Stainless steels | ≤ 0.08 | 18 |
| 12Х17Г9АН4 | 1.3965 | Non-magnetic steels | ≤ 0.1 | 9 |
| 12Х17Г9АН4 | 1.4372 | Others | ≤ 0.15 | 10 |
| 12Х17Г9АН4 | 1.4373 | Non-magnetic steels | ≤ 0.15 | 13 |
| 12Х18Н10Т | 1.4878 | Heat resistant steels | ≤ 0.1 | 14 |
| 12Х18Н10Т | 1.4541 | Stainless steels | ≤ 0.08 | 25 |
| 12Х18Н12 | 1.4303 | Stainless steels | ≤ 0.06 | 14 |
| 12Х18Н12М3ТЛ | 1.4581 | Cast stainless steels | ≤ 0.07 | 9 |
| 12Х18Н9 | 1.4300 | Stainless steels | ≤ 0.12 | 15 |
| 12Х18Н9Т | 1.4541 | Stainless steels | ≤ 0.08 | 25 |
| 12Х18Н9ТЛ | 1.4312 | Cast stainless steels | ≤ 0.12 | 15 |
| 12Х19Н7Г2САЛ | — | — | ≤ 0.12 | — |
| 12Х1МФ | 1.7715 | Heat-resistant structural steels | 0.1–0.18 | 8 |
| 12Х1МФ | — | — | 0.08–0.15 | 1 |
| 12Х21Н5Г2САЛ | — | — | ≤ 0.12 | — |
| 12Х21Н5Г2СЛ | — | — | ≤ 0.12 | — |
| 12Х21Н5Г2СМ2Л | — | — | ≤ 0.12 | — |
| 12Х21Н5Г2СТЛ | — | — | ≤ 0.12 | — |
| 12Х21Н5Т | — | — | 0.09–0.14 | — |
This grade’s own name — recorded in our sources as this grade’s own designation under that standard.
Indicative — taken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawn — designation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.