Every grade designated under GOST, with the material number it maps to, what kind of steel it is, its carbon window and how many other standards carry it. Open a grade for its full composition, properties and its designations in other standards. Every name on this page is an indicative cross-reference, not an asserted identity: the grades are close, not interchangeable. Check the composition before you substitute.
Also known as
3544 designations| Grade | Material no. | Category | C% by weight | Also inother standards |
|---|---|---|---|---|
| АS40KHGNM | 1.0501 | Quenched and tempered steels | 0.32–0.39 | 23 |
| АS45G2 | 1.0912 | Others | 0.42–0.5 | 11 |
| АSTS30KHM | 1.0528 | Quenched and tempered steels | 0.27–0.34 | 14 |
| АTS20KHGNM | 1.1152 | Cold extrusion steels | 0.18–0.22 | 4 |
| АС11 | — | — | 0.07–0.15 | — |
| АС14 | — | — | 0.1–0.17 | — |
| АС14ХГН | — | — | 0.13–0.18 | — |
| АС19ХГН | — | — | 0.16–0.21 | — |
| АС38ХГМ | 1.7220 | Quenched and tempered steels | 0.3–0.37 | 24 |
| АЧВ-1 | — | — | 2.8–3.5 | — |
| АЧК-1 | — | — | 2.3–3 | — |
| АЧС-1 | — | — | 3.2–3.6 | — |
| АЧС-4 | — | — | 3–3.5 | — |
| ВКЛ-1 | 1.0035 | Unalloyed structural steels | — | 22 |
| ВНЛ-1 | — | — | ≤ 0.08 | — |
| ВНЛ-2 | 1.0308 | Unalloyed structural steels | ≤ 0.17 | 10 |
| ВНЛ-3 | 1.0116 | Unalloyed structural steels | ≤ 0.17 | 12 |
| ВНЛ-4 | 1.0040 | Unalloyed structural steels | ≤ 0.25 | 8 |
| ВНС-2-Ш | 1.0308 | Unalloyed structural steels | ≤ 0.17 | 10 |
| ВСт4кп | 1.0040 | Unalloyed structural steels | ≤ 0.25 | 8 |
| ВСт5пс | 1.0507 | Others | ≤ 0.2 | 8 |
| ВЧ100 | — | — | 3.2–3.6 | — |
| ВЧ40 | EN-JS1030 | Others | — | 17 |
| ВЧ40 | EN-JS1072 | Others | — | 17 |
| ВЧ40 | EN-JS1073 | Others | — | 17 |
| ВЧ50 | EN-JS1082 | Others | — | 20 |
| ВЧ50 | EN-JS1083 | Others | — | 20 |
| ВЧ60 | EN-JS1060 | Others | — | 20 |
| ВЧ60 | EN-JS1092 | Others | — | 20 |
| ВЧ60 | EN-JS1093 | Others | — | 20 |
| ВЧ70 | EN-JS1102 | Others | — | 21 |
| ВЧ70 | EN-JS1103 | Others | — | 21 |
| ВЧ80 | EN-JS1080 | Others | — | 16 |
| Г13А | — | — | 1–1.2 | — |
| ДИ-13 | — | — | ≤ 0.1 | — |
| ДИ-21 | — | — | ≤ 0.08 | — |
| ДИ-77 | — | — | ≤ 0.08 | — |
| ДИ1 | 1.0035 | Unalloyed structural steels | — | 22 |
| ДИ1-Ш | 1.0035 | Unalloyed structural steels | — | 22 |
| ДИ100-МП | — | — | 3.2–3.6 | — |
| ДИ101-МП | 1.3243 | High-speed steels | 0.87–0.95 | 19 |
| ДИ102-МП | 1.3207 | High-speed steels | 1.2–1.35 | 14 |
| ДИ103-МП | — | — | 1.05–1.15 | — |
| ДИ22 | 1.2567 | Tool steels for hot work | 0.25–0.35 | 9 |
| ДИ23 | — | — | 0.45–0.52 | — |
| ДИ32 | — | — | 0.46–0.53 | — |
| ДИ37 | — | — | 1.05–1.15 | — |
| ДИ55 | — | — | 0.85–0.95 | — |
| ДИ59 | — | — | 0.06–0.1 | — |
| ДИ70-МП | EN-JS1102 | Others | — | 21 |
This grade’s own name — recorded in our sources as this grade’s own designation under that standard.
Indicative — taken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawn — designation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.