SCCrM1
The designation SCCrM1 is carried by 3 different grades. Compare them on the elements that actually differ, then open the one your print means.
Which of the 3 do you want?
This name is carried by several grades. The elements shown are the ones whose values actually differ across the set — the ones that decide the question. Values are the source text verbatim; an em dash means no value on file for that element on that grade, not zero.
| Grade | Material no. | Category | Designations | C% | P% | Si% | S% | Cr% | Mn% |
|---|---|---|---|---|---|---|---|---|---|
| 1.7218 | 1.72181.7 | Quenched and tempered steels | 111 | 0,22-0,29 | 0,025 | ≤0,40 | 0,035 | 0,90-1,20 | 0,60-0,90 |
| 1.7220 | 1.72201.7 | Quenched and tempered steels | 159 | 0,30-0,37 | 0,035 | ≤0,40 | 0,035 | 0,90-1,20 | 0,60-0,90 |
| sccrm1 | — | Cast steel | 1 | 0.2 - 0.3 | max 0.04 | 0.3 - 0.6 | max 0.04 | 0.8 - 1.2 | 0.5 - 0.8 |
Not sure which one your print means?
Search the catalogue by designation, material number or composition — every name on this page is itself a way in.