| Grade | Material no. | Category | Designations | C% | Si% | P% | S% | Cr% | Mn% |
|---|---|---|---|---|---|---|---|---|---|
| 1.7218 | 1.72181.7 | Quenched and tempered steels | 111 | 0,22-0,29 | ≤0,40 | 0,025 | 0,035 | 0,90-1,20 | 0,60-0,90 |
| scm425 | — | 1 | 0.23 - 0.28 | 0.15 - 0.35 | max 0.03 | max 0.03 | 0.9 - 1.2 | 0.6 - 0.9 | |
| 25CrMo4 | — | 4 | 0.23-0.28 | 0.1-0.3 | ≤0.025 | ≤0.025 | 0.9-1.2 | 0.6-0.9 |