G43400
The designation G43400 is carried by 4 different grades. Compare them on the elements that actually differ, then open the one your print means.
- Matching grades 4
- Category Quenched and tempered steels · 133 grades
Which of the 4 do you want?
This name is carried by several grades. The elements shown are the ones whose values actually differ across the set — the ones that decide the question. Values are the source text verbatim; an em dash means no value on file for that element on that grade, not zero.
| Grade | Material no. | Category | Designations | C% | Cr% | Ni% | Mo% | Mn% | Si% |
|---|---|---|---|---|---|---|---|---|---|
| 1.6511 | 1.65111.6 | Quenched and tempered steels | 91 | 0,32-0,40 | 0,90-1,20 | 0,90-1,20 | 0,15-,30 | 0,50-0,80 | ≤0,40 |
| 40NiCrMo6 | 1.65651.6 | Quenched and tempered steels | 56 | 0,35-0,45 | 0,90-1,40 | 1,40-1,70 | 0,20-0,30 | 0,50-0,70 | 0,15-0,35 |
| 30CrNiMo8 | 1.65801.6 | Quenched and tempered steels | 29 | 0,26-0,34 | 1,80-2,20 | 1,80-2,20 | 0,30-0,50 | 0,30-0,60 | ≤0,40 |
| 1.6582 | 1.65821.6 | Quenched and tempered steels | 84 | 0,30-0,38 | 1,30-1,70 | 1,30-1,70 | 0,15-0,30 | 0,50-0,80 | ≤0,40 |
Not sure which one your print means?
Search the catalogue by designation, material number or composition — every name on this page is itself a way in.