SteelEquivalents.com

Explore

MaterialsSteel materials by standardCategoriesSteel material categoriesSearchSteel grade searchCalculatorsSteel calculatorsServicesCutting, machining and finishing to order
Latest news
Knowledge & SafetySteel WikiGrades, standards and metallurgy explained
Help & SupportContactGet in touch with the teamFAQCommon questions answeredSupport Chat pageFAQs, guides & live chat in one place
Settings

Appearance

Accent

Language

Welcome

Sign in to save favorites and manage your account.

MSZ · Hungary · 49 designations

K13K

K13K is a designation in MSZ for the material held under material number 1.2344, also listed as X40CrMoV5-1. It is a material in the category Tool steels for hot work. We list 49 designations recorded for this grade, in the standards DIN / EN, UNS, AISI / SAE, BS, AFNOR, UNE, ISO, JIS, GB, GOST, UNI, SS, ČSN, STN, SRPS, PN, MSZ, STAS, BDS, ÖNORM and KS.

If you came for one of these

The most-used names for this grade.

About Tool steels for hot work

Tool steels for hot work are alloy steels designed for tooling that operates in contact with heated metal. They are characterised by hot hardness, wear resistance, toughness and resistance to thermal fatigue, making them suitable for dies, moulds, punches and other forging, extrusion and die-casting tools.

This describes the material class as a whole. Always confirm the individual grade against the standard before ordering.

Also known as

49 designations · 21 standards · nothing hidden
This grade’s own namerecorded in our sources as this grade’s own designation under that standard.
Indicativetaken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawndesignation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.

Every designation on file is listed — no truncation, no “+ n more”. Each one is itself a route that leads back here.

Chemical composition

8 elements on file · weight %

What this alloy is

Iron — the balance, never listed by a standard — 90.7 %Cr — 5.2 %Mo — 1.4 %Si — 1 %Traces & impurities · 1.8 %

Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.

Element% by weight
0.35–0.42
0.8–1.2
0.25–0.5
0.03
0.02
4.8–5.5
1.2–1.5
0.85–1.15
CarbonSiliconManganesePhosphorusSulfurChromiumMolybdenumVanadium
0.01 %0.1 %1 %10 %100 %

The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.

ElementAs publishedsource text, verbatimMin% by weightMax% by weightBound
C0,35-0,420.3500.420Range
Si0,80-1,200.8001.200Range
P0,030.0300.030Exact
S0,020.0200.020Exact
V0,85-1,150.8501.150Range
Cr4,80-5,504.8005.500Range
Mn0,25-0,500.2500.500Range
Mo1,20-1,501.2001.500Range

The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.

Predicted transformation temperatures

Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.

Physical & mechanical properties

Density7,78g/cm³Exact
Transformation point Ac1875°CExact
Transformation point Ac3935°CExact · Ac3(Acm)
Transformation point Ar3815°CExact · Ar3(Arcm)
Transformation point Ar1760°CExact

An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.

Properties by condition

5 conditions · 42 values
By delivery stateno delivery state statedsource steeljis
Delivery stateHBHRC
Annealed229
Quenched and tempered50
By delivery stateSoft annealedsource steelnumber
Delivery stateHB
Soft annealed229
By heat-treated conditionno delivery state statedsource splav
Heat-treated conditionRmN/mm²ReN/mm²A5%Z%KCUkJ/m²
Quenching 1020°C, oil, Drawing 580°C, 2h167014701040390
By delivery stateno delivery state statedsource splav
Delivery stateHB
4KH5MF1S ( 4Х5МФ1С ) (annealing) , GOST 5950-2000241
At temperatureno delivery state statedsource splav
Temperature°CDensityg/cm³Elastic modulusGPaThermal conductivityW/(m·K)Electrical resistivitynΩ·m
207.71620722553
1007.69225591
2007.6627649
3007.62718729715
4007.59330793
5007.55931879
6007.52316031970
7007.49311077
8007.459311189
9007.438321229

Every figure holds only for the condition on its own row. Values are never merged across conditions or across sources, never averaged, and never interpolated between two rows. An em dash means no value on file — never zero. Figures are converted to the unit in the column header; the source’s own wording is kept and shown where the two differ.

Heat treatment

Supply condition

  • QuenchingTest specimen
  • AnnealingSupply condition

Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.

Source: www.caishuku.com

Similar grades — and why

Selection rule, stated so you can disagree with it: same number class 1.2, a shared category, and a published range for Cr / Mo that overlaps this grade’s. These are neighbours in composition space — they are not equivalents, and none is claimed to be interchangeable with this grade.

Looking for this grade under another name?

Search the catalogue by designation, material number or composition — every name on this page is itself a way in.