Every grade designated under PN, with the material number it maps to, what kind of steel it is, its carbon window and how many other standards carry it. Open a grade for its full composition, properties and its designations in other standards. Every name on this page is an indicative cross-reference, not an asserted identity: the grades are close, not interchangeable. Check the composition before you substitute.
Also known as
635 designations| Grade | Material no. | Category | C% by weight | Also inother standards |
|---|---|---|---|---|
| H25N20S2 | 1.2782 | Tool steels for hot work | ≤ 0.2 | 6 |
| H25N21 | 1.4845 | Heat resistant steels | ≤ 0.1 | 21 |
| H25T | 1.4749 | Heat resistant steels | 0.15–0.2 | 10 |
| H25T | 1.4746 | Others | ≤ 0.12 | 8 |
| H26N4 | 1.4821 | Heat resistant steels | 0.1–0.2 | 3 |
| H5M | 1.7362 | Hydrogen resistant steels | 0.1–0.15 | 13 |
| H5M | 1.7366 | Others | ≤ 0.18 | 6 |
| H6S2 | 1.4713 | Heat resistant steels | ≤ 0.12 | 7 |
| H6S2 | 1.4712 | Heat resistant steels | ≤ 0.12 | 3 |
| H9S2 | 1.4718 | Valve steels | 0.4–0.5 | 16 |
| H9S2 | 1.4718 | Others | 0.4–0.5 | 16 |
| K10 | 1.0301 | Case hardening steels | 0.07–0.13 | 20 |
| K18 | 1.0402 | Quenched and tempered steels | 0.17–0.24 | 24 |
| K18 | 1.0436 | Fine-grain structural steels | 0.15–0.2 | 14 |
| K32Nb | 1.6368 | Heat-resistant structural steels | ≤ 0.17 | 4 |
| K32NbA | 1.6368 | Heat-resistant structural steels | ≤ 0.17 | 4 |
| L120G13 | 1.3401 | Quenched and tempered steels | 1.1–1.3 | 19 |
| L18HM | 1.7733 | Heat-resistant structural steels | 0.2–0.28 | 15 |
| L20 | 1.0443 | Others | ≤ 0.11 | 13 |
| L20G | 1.1120 | Others | 0.17–0.23 | 13 |
| L210H21 | 2.4066 | Nickel and cobalt alloys | ≤ 0.1 | 10 |
| L210H21 | 2.4068 | Nickel and cobalt alloys | ≤ 0.02 | 8 |
| L25HM | 1.7220 | Quenched and tempered steels | 0.3–0.37 | 24 |
| L25HM | 1.7218 | Quenched and tempered steels | 0.22–0.29 | 25 |
| L35G | 1.1167 | Quenched and tempered steels | 0.32–0.4 | 17 |
| L35HM | 1.7220 | Quenched and tempered steels | 0.3–0.37 | 24 |
| L400 | 1.0416 | Others | 0.15–0.2 | 17 |
| L40H5MF | 1.2344 | Tool steels for hot work | 0.35–0.42 | 20 |
| L450 | 1.0443 | Others | ≤ 0.11 | 13 |
| L500 | 1.0552 | Others | ≤ 0.25 | 13 |
| LH14 | 1.4027 | Cast stainless steels | 0.16–0.23 | 14 |
| LH15 | 1.3505 | Bearing steels | 0.93–1.05 | 22 |
| ŁH15 | 1.3505 | Bearing steels | 0.93–1.05 | 22 |
| ŁH15 | 1.2067 | Tool steels for cold work | 0.95–1.1 | 21 |
| LH15 | 1.2067 | Tool steels for cold work | 0.95–1.1 | 21 |
| LH15SG | 1.3520 | Bearing steels | 0.93–1.05 | 16 |
| ŁH15SG | 1.3520 | Bearing steels | 0.93–1.05 | 16 |
| LH18N9 | 1.4312 | Cast stainless steels | ≤ 0.12 | 15 |
| LH18N9T | 1.4312 | Cast stainless steels | ≤ 0.12 | 15 |
| LH23N18C | 1.4826 | Heat-resistant cast steels | 0.3–0.5 | 13 |
| LH25N19S2 | 1.4848 | Heat-resistant cast steels | 0.3–0.5 | 10 |
| LII400 | 1.0416 | Others | 0.15–0.2 | 17 |
| LII400 | 1.0443 | Others | ≤ 0.11 | 13 |
| LII500 | 1.0551 | Unalloyed structural steels | ≤ 0.24 | 10 |
| LII500 | 1.0552 | Others | ≤ 0.25 | 13 |
| LOH13 | 1.4006 | Stainless steels | 0.08–0.15 | 26 |
| MSt5 | 1.0050 | Unalloyed structural steels | — | 23 |
| MSt5 | 1.0050 | Unalloyed structural steels | — | 23 |
| MSt6 | 1.0060 | Unalloyed structural steels | — | 21 |
| MSt6 | 1.0060 | Unalloyed structural steels | — | 21 |
This grade’s own name — recorded in our sources as this grade’s own designation under that standard.
Indicative — taken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawn — designation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.