SteelEquivalents.com

Explore

MaterialsSteel materials by standardCategoriesSteel material categoriesSearchSteel grade searchCalculatorsSteel calculatorsServicesCutting, machining and finishing to order
Latest news
Knowledge & SafetySteel WikiGrades, standards and metallurgy explained
Help & SupportContactGet in touch with the teamFAQCommon questions answeredSupport Chat pageFAQs, guides & live chat in one place
Settings

Appearance

Accent

Language

Welcome

Sign in to save favorites and manage your account.

STAS · Romania · 28 designations

T20Cr130

T20Cr130 is a designation in STAS for the material held under material number 1.4027, also listed as GX20Cr14. It is a material in the category Cast stainless steels. We list 28 designations recorded for this grade, in the standards DIN / EN, AISI / SAE, BS, AFNOR, UNE, JIS, GB, GOST, UNI, ČSN, PN, MSZ, STAS, BDS and KS.

If you came for one of these

The most-used names for this grade.

About Cast stainless steels

Cast stainless steels are stainless-steel materials produced by casting, combining corrosion resistance with the ability to form complex component shapes. Their composition and mechanical behaviour vary by grade, and they are used for corrosion-resistant cast components such as pumps, valves and process equipment.

This describes the material class as a whole. Always confirm the individual grade against the standard before ordering.

Also known as

28 designations · 15 standards · nothing hidden
This grade’s own namerecorded in our sources as this grade’s own designation under that standard.
Indicativetaken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawndesignation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.

Every designation on file is listed — no truncation, no “+ n more”. Each one is itself a route that leads back here.

Chemical composition

7 elements on file · weight %

What this alloy is

Iron — the balance, never listed by a standard — 83.2 %Cr — 13.5 %Si — 1 %Mn — 1 %Traces & impurities · 1.3 %

Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.

Element% by weight
0.16–0.23
≤ 1
≤ 1
0.045
0.03
12.5–14.5
1
CarbonSiliconManganesePhosphorusSulfurChromiumNickel
0.01 %0.1 %1 %10 %100 %

The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.

ElementAs publishedsource text, verbatimMin% by weightMax% by weightBound
C0,16-0,230.1600.230Range
Si≤1,001.000Max
P0,0450.0450.045Exact
S0,030.0300.030Exact
Cr12,5-14,512.50014.500Range
Mn≤1,001.000Max
Ni11.0001.000Exact

The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.

Predicted transformation temperatures

Not enough recorded composition to predict a transformation temperature for this grade — missing: Mo.

Physical & mechanical properties

Density7,85g/cm³Exact
Weldabilityweldable with restrictionsAs published: limited weldability.

An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.

Properties by condition

3 conditions · 58 values
By delivery stateno delivery state statedsource steeljis
Delivery stateRmN/mm²ReN/mm²A%Z%HB
Casting5903901635
Quenched and tempered170 – 235
By dimensionno delivery state statedsource splav
DimensionmmRmN/mm²ReN/mm²A5%Z%KCUkJ/m²
to 1005894411640392
At temperatureno delivery state statedsource splav
Temperature°CDensityg/cm³Elastic modulusGPaThermal expansion coefficient10^-6/KThermal conductivityW/(m·K)Specific heat capacityJ/(kg·K)Electrical resistivitynΩ·m
207.7422221645
1002161023470695
20021110.824491775
30020311.325512859
40019511.726533931
50018412.127563985
60016712.4275961055
70014912.6276431115
80014012.8286801125
90010.8286931160

Every figure holds only for the condition on its own row. Values are never merged across conditions or across sources, never averaged, and never interpolated between two rows. An em dash means no value on file — never zero. Figures are converted to the unit in the column header; the source’s own wording is kept and shown where the two differ.

Heat treatment

GB 2100-1980

Choose one
  • A · Annealing950 °C
  • B · Quenching1050 °C
    Quenchant Oil or Air

Source: www.caishuku.com

Similar grades — and why

Selection rule, stated so you can disagree with it: same number class 1.4, a shared category, and a published range for Cr / Ni that overlaps this grade’s. These are neighbours in composition space — they are not equivalents, and none is claimed to be interchangeable with this grade.

Looking for this grade under another name?

Search the catalogue by designation, material number or composition — every name on this page is itself a way in.