SteelEquivalents.com

Explore

MaterialsSteel materials by standardCategoriesSteel material categoriesSearchSteel grade searchCalculatorsSteel calculatorsServicesCutting, machining and finishing to order
Latest news
Knowledge & SafetySteel WikiGrades, standards and metallurgy explained
Help & SupportContactGet in touch with the teamFAQCommon questions answeredSupport Chat pageFAQs, guides & live chat in one place
Settings

Appearance

Accent

Language

Welcome

Sign in to save favorites and manage your account.

UNE · Spain · 14 designations

F.1741

F.1741 is a designation in UNE for the material held under material number 1.8507, also listed as 34CrAlMo5-10. It is a material in the category Nitriding steels. We list 14 designations recorded for this grade, in the standards DIN / EN, UNS, AISI / SAE, BS, AFNOR, UNE, GOST, PN and SRPS.

If you came for one of these

The most-used names for this grade.

About Nitriding steels

Nitriding steels are alloy steels designed for nitriding, a surface-hardening treatment that produces a hard, wear-resistant surface while retaining a tough supporting core. They are used for gears, shafts, dies and other components requiring resistance to wear, repeated loading and dimensional change in service.

This describes the material class as a whole. Always confirm the individual grade against the standard before ordering.

Also known as

14 designations · 9 standards · nothing hidden
This grade’s own namerecorded in our sources as this grade’s own designation under that standard.
Indicativetaken from a published cross-reference table; a close match, not a guarantee of interchangeability. Verify against the mill certificate before ordering.
Withdrawndesignation no longer current — a separate column from the two above, so a name can be same grade and withdrawn at once.

Every designation on file is listed — no truncation, no “+ n more”. Each one is itself a route that leads back here.

Chemical composition

8 elements on file · weight %

What this alloy is

Iron — the balance, never listed by a standard — 96.3 %Cr — 1.2 %Al — 1 %Mn — 0.6 %Traces & impurities · 1 %

Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.

Element% by weight
0.3–0.37
≤ 0.4
0.4–0.7
0.025
0.035
1–1.3
0.15–0.25
0.8–1.2
CarbonSiliconManganesePhosphorusSulfurChromiumMolybdenumAluminium
0.01 %0.1 %1 %10 %100 %

The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.

ElementAs publishedsource text, verbatimMin% by weightMax% by weightBound
C0,30-0,370.3000.370Range
Al0,80-1,200.8001.200Range
Si≤0,400.400Max
P0,0250.0250.025Exact
S0,0350.0350.035Exact
Cr1,00-1,301.0001.300Range
Mn0,40-0,700.4000.700Range
Mo0,15-0,250.1500.250Range

The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.

Predicted transformation temperatures

Not enough recorded composition to predict a transformation temperature for this grade — missing: Ni.

Physical & mechanical properties

Density7,85g/cm³Exact

An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.

Properties by condition

2 conditions · 5 values
By thicknessQuenched and temperedsource steelnumber
ThicknessmmRmN/mm²A%
16 – 40800 – 100014
40 – 100800 – 100014
By delivery stateSoft annealedsource steelnumber
Delivery stateHB
Soft annealed248

1 further values are held for this grade under a condition the source did not name — a bound with no quantity attached. They are withheld rather than shown against a guessed condition.

Every figure holds only for the condition on its own row. Values are never merged across conditions or across sources, never averaged, and never interpolated between two rows. An em dash means no value on file — never zero. Figures are converted to the unit in the column header; the source’s own wording is kept and shown where the two differ.

Heat treatment

Supply condition

  • Nitriding
  • Soft annealingBar, Rod, Flat product, Forging and Semi-finished product
  • Quenching and TemperingBar, Flat product and Forging16≤d≤40
  • Quenching and Tempering16≤d≤1008≤t≤60

Conditions the standard permits on delivery. No temperature or medium is published for these, so no order and no alternation is implied.

Source: www.caishuku.com

Similar grades — and why

Selection rule, stated so you can disagree with it: same number class 1.8, a shared category, and a published range for Cr / Al that overlaps this grade’s. These are neighbours in composition space — they are not equivalents, and none is claimed to be interchangeable with this grade.

Looking for this grade under another name?