KS · South Korea · 1 designation

SK95-CSP

SK95-CSP is a material in the category Spring steels. Its recorded composition includes C 0.9–1%, Si ≤ 0.35%, Mn ≤ 0.5%, Ni ≤ 0.25% and Cu ≤ 0.3%. No cross-standard equivalents are recorded for this grade yet. Recorded mechanical properties include HV 200.

About Spring steels

Spring steels are alloy steels designed to store and release elastic energy repeatedly without permanent deformation. They are characterised by a combination of strength, hardness and resilience, making them suitable for springs, clips, washers and other components subjected to repeated flexing or shock.

This describes the material class as a whole. Always confirm the individual grade against the standard before ordering.

Chemical composition

8 elements on file · weight %

What this alloy is

Iron — the balance, never listed by a standard — 97.4 %C — 1 %Mn — 0.5 %Si — 0.4 %Traces & impurities · 0.8 %

Logarithmic scale, 0.01 % to 100 % — every value here compares directly, decade by decade.

Element% by weight
0.9–1 —
≤ 0.35
≤ 0.5
≤ 0.03
≤ 0.03
≤ 0.2
≤ 0.25
≤ 0.3
CarbonSiliconManganesePhosphorusSulfurChromiumNickelCopper
0.01 %0.1 %1 %10 %100 %

The scale is logarithmic, not the element’s raw share of the alloy — the only honest way to fit 0.01 % and 100 % in one picture, and it means every value here can be compared with every other.

ElementAs publishedsource text, verbatimMin% by weightMax% by weightBound
C0.9 - 10.9001.000Range
Simax 0.350.350Max
Pmax 0.030.030Max
Smax 0.030.030Max
Crmax 0.20.200Max
Mnmax 0.50.500Max
Nimax 0.250.250Max
Cumax 0.30.300Max

The published column is the source string byte-for-byte, decimal comma and all; Min and Max are the parsed bounds. Elements not listed have no value on file — they are omitted, never inferred.

Predicted transformation temperatures

Not enough recorded composition to predict a transformation temperature for this grade — missing: Mo.

Physical & mechanical properties

An absent property means we hold no value for it — it is left out rather than estimated, interpolated from a neighbouring grade, or filled from a handbook. It does not mean the property is undefined for the material.